Default ano outcome with no dye

Just curious........

When I dont use dye, my parts come out with more of a greyish color as compared to parts I can buy that are "silver" ano'd. I compared to a couple different parts from different places, so I dont think that they are all bright dipping.

I heavily polish, use caswells cleaner and desmut before ano. Any ideas on why my parts arent as silver?