Okay here is the deal folks. I got my oven finished or at least I think I did. I placed a motorcycle wheel and swing arm in the oven to pre-heat for out gassing. I thought I would keep an eye on the temp of the parts to see how long it would take for them to get to 400. After around 35min the parts never reached the temp. They got to around 350 in one spot, but an inch below the 350 spot it was 314 and in a other section it was 287. I am not sure if the ir temp probe works that great or it’s something else. Just wanted to see if any one out there has had the same problem. Just so you know the oven was set to 400 and reached the temp. If you have done a motorcycle how long did you have it in the oven for?