Thread: IR Temp Probes
View Single Post
  #1 (permalink)  
Old 07-19-2004, 08:01 PM
getastro's Avatar
getastro getastro is offline
Amateur Metal Finisher
 
Join Date: May 2003
Location: NSB, FL.
Posts: 59
getastro
Default IR Temp Probes

Hello all, early on in the week I asked about parts getting up to correct temperature in the oven. Well, I was using a Mini-Temp IR hand held device to find the part temp. I was not positive that I was getting the right temp. So after speaking to a person who deals with temperature measurement, he told me that the IR devices are the wrong things to use. It seems that the color of the part you coated and the heat of the oven or light can cause the IR device to give you a wrong temp. He told me to use a surface probe hooked Multi-meter type device. This would give you the correct measurement and color or surrounding heat won’t affect it. Just wanted to let folks know.
Reply With Quote