I'm new to this forum, so please bear with me a moment while I describe my problem. Maybe one of you can help me out. I have no problem with the first three steps. Flash copper, acid copper and nickle. All the steps are done by the numbers and they come out great. Then when I get to the chrome tank, everything goes crazy. Again, I'm trying to do it exactly by the numbers but maybe I'm missing something. I have the anodes (2) placed in the tank with a jumper wire connecting them. The part I'm trying to plate is small, so the anodes are aprox. five inches apart. The part is a 2x2 angle iron 2" long. Therefore the amps are set at 16 amps. + to the anode and - to the part. Within a few minutes of being in the chrome tank, the nickle is stripped and sometimes some of the copper. It seems to be more severe were the wire hook is attached. I thought that maybe the batch was bad so I mixed up a new batch, but still the same thing. I've been back and forth with the tech. dept. for a couple of days now but we can't seem to figure it out. While I'm on this subject, exactly how critical is the amp settings. (+ or -). I now have a digital amp meter set up so I can get it right on the button. I sure would appreciate any help you could offer as I'm about to lose my mind.