Negative! I'm absolutely sure the polarity is correct. I've checked them a couple of times and had 4 others check it out also. I thought the same thing. As it turns out, I managed with little effort to get my first chromed piece this afternoon. YEAH!!! The first thing this morning I went to Home Depot and bought bare copper ground wire to hang the part by. Much larger than the #10 copper I was using. Then I hooked it by two spots rather than one. I also picked up heavy duty clips and some #6 stranded wire (black & red). I minimized the resistance as much as possible. It seems to have done the trick. The most damage was always at the point of contact with the hanger. Maybe I was burning it off, ya think? I do however get some foam around the work piece area Not a lot though. Is that a bad thing?