Default Powder Coating bake off fumes?

Hi:
Been a long time PC hobbist, I am in the process of going in a commercial PC venture. I plan to do small batch PC work focused on the Auto, Motorcycle & boating enthuaist. My local fire dept. has some concerns of the Bake off fumes being flammable. Is their some info available on line I can download to pursaude the fire dept. to approve my permit?
Thanks
Bob