For "haze" removal, ease up on your pressure a bit. I did a large, flat skidplate a few weeks ago that was good but for the "haze". I loaded up a loose wheel with white roughe and let it just barely glide over the surface. All the haze went away.
I was able to duplicate this success on the skid plate's billet clamps as well..
|