Quote:
|
Originally Posted by wc1971
Has anyone powdercoated clear over copper plating? I am wondering if it would dull the copper? Also does anyone have photos of anything done in a copper color powder?
Thanks
|
I've done clear over 110 copper. No pictures, but it works fine. Just make sure you get good coverage on the first coat, else the copper will oxidize in the oven (turn reddish).