High temp silver discoloring
View Single Post
#
6
(
permalink
)
07-26-2004, 11:08 PM
Noob2PC
Experienced Metal Finisher
Join Date: Mar 2004
Location: Greensboro NC
Posts: 315
Did you Prebake it after sandblasting
? I know that I have to do that or my powder looks like dodo! I have some Valve covers that I have blasted and prebaked 2 times already and I plan on prebaking/outgassing at least one more time.