after you out gas clean it again . and the oil from your fingers will show if not cleaned off . i wear rubber toss away gloves when handling all part's ... from what i found about alum. it has alot of little pores and the mixture is not the best on some part's .. the usa part's and coarse and the jap part's are nice to work on
|