The pipe was clean as in the pics even after baking, if the discoloration is from oil, then it came after the final bake while installing and using. The part is going to get dirty during use, and if it's that oil burning there is no way around it. This stuff in person looks like the actual powder is discoloring when you look at it, almost like it's rusting.