View Single Post
  #5 (permalink)  
Old 07-27-2004, 01:22 AM
customandsound
Guest
 
Posts: n/a
Default

clean with simple green and hot water .. wear rubber glove's change for each compound and rake the buff's out til they are fluffy
Reply With Quote