Thread
:
High temp silver discoloring
View Single Post
#
10
(
permalink
)
07-27-2004, 01:25 AM
customandsound
Guest
Posts: n/a
if it is powder form caswell contact them ... you may need to use tech line of it i know them little motors let out some heat ...
customandsound