\"If you strip off the chrome with sandblasting, you will have gotten to the nickel\"

Wouldn\'t I have gotten to the pot metal?

I was planning on filling the pits with Solder-It, but I have had ZERO succes with this stuff and am very frustrated. I can\'t get it to \"take\" to any pot metal parts; parts that contain zinc as they \"fizz\" with the application of acid.

I plan on stripping, pot metal priming, then copy chrome plating.... but haven\'t had much luck so far.