Re: Solder-NOT !?
Put it in the oven to heat up the entire part before trying to solder it.
The problem you describe is a problem familiar to us, and heating the part in an oven first tends to solve it.
Usually, heating with a torch doesn\'t work as well. Perhaps the part is only heated locally.
|