View Single Post
  #1 (permalink)  
Old 08-03-2004, 11:02 PM
plater12 plater12 is offline
Newbie
 
Join Date: Jun 2004
Posts: 6
plater12
Default what plating machine

am doing some copper plating with a caswell kit,it is a 2
> gallon
> > plastic bucket ,i tried it with a very small hr machine and it
> did
> > not work,maybee its broken?,i hooked it up to a 12 volt car
> battery
> > with one bulb on there and it worked ok but i would prefer a
> plating
> > machine that would work,i want to use it for gold plate and
> nickel
> > also,any one have any suggestions on a plating machine to
> get.Thanks
Reply With Quote