Noob here,
I'm finishing a four foot tall sculpture , which I hope to PC this weekend. I an effort to cover up a fair amount of deep scratches and mis-weldings I plan to use JB Weld. I tried a sample earlier today and found it covered well and flowed normally ( 400 for 25 min.) I noticed in searching the archives that the consensus is not to use it though my destructive tests showed a tight bond and no noticeable disintegration of the JB Weld. So...Comments, do I trust it?
Thanks
Dick