I just ordered a Copy Chrome PNP kit, as well as some Black Chrome and Copper PNP refills with some extra wands...

It says Copy Chrome PNP will plate directly to steel. Will my results be better if I plate first with copper?

Also, should I still get the degreaser kit to do wand plating? Or will any degreaser/solvent work ok?

How thick can I build the layers with the wand? I mean if I keep brushing on new layers, will it keep getting thicker? (without having to "pickle" the surface between coats)

thanks

Jon