Lloyd, thanks for your reply. We are exclusively doing brush plating so measuring the copper wire is not an option at this stage. Good idea though.

So far, we are assuming an anode efficiency of approx 90% and we deduce the plate thickness according to the time spent plating; not a very accurate method unfortunately. Although with this method we are pretty certain that we achieve at least a certain thickness, we are not exactly sure as to how much.

Regards,

Ares