it is not shiney at all it came out looking more like a grey/silver any ideas why? i was thinking maybe too thick? i baked it at 375 for 25 minutes and it looked the same the whole time. also i sprayed trans. blue over it and it seemed to not be thick enough in some spots and didnt cover so well. what would happen if i put another coat of blue on would it look bad because it is trans. ? thank for any advice.... randy