When doing the trans. candy colors we found it best to bake the chrome for 15 min then shot it with the trans color when it starts to cool around 150 deg. Even prior parts that were chromed weeks ago, still coat great with the trans color. Trick is, in my opinion, shot will still warm. We been having great results with the candies doing it this way. Hope it helps.
|