How is it going?
Well I have had a chance to do quite a bit of platting and thanks again for your suggestions on using the resistor to start the power supply. It even helps to start the unit in the flash copper with low current settings. I understand you get what you pay for, but, I wonder if I have a "special" unit or all of the "HY3020E" units like this? Does anyone else have to use a resistor to get their power supply to start? I have quite a selection of resistors now and I just don't seem to think this is what I should "need" to do. P.S. I am getting better at the math too, LOL.
Do you know of anyone else who has purchased one of these units ?
And are they encountering the same problem?