Quote:
|
Originally Posted by pdeinc
NoobPC, be careful with coat hangers, they're coated and will have to be stripped to make good contact. Welding rod would be easier, altho not as available to everyone.
|
I am aware of that, it is easier to sand paper off the zinc coating then the accumulated Powder