Don't over look buying hooks. I pay between $10.00 and $15.00 per thousand hooks depending on size. Then I throw them away after single use. They are always clean and grounded.The customers don't realize the .10 to .15 cents built into the price of the coating job.When you figure your time to strip or make hooks versus paying for them it works out very close to equal. Then the saved time can be spent coating more pieces for higher income. Some of you will say "1000 hooks will take forever to use up that many", they go faster than you think.
|