Thanks!

I've been trying to get my info from a number of places but yet mostly on the Net - a but unfortunately it seems - I do have some books coming in the next couple of days so that should help.

I don't care what method it is as long as it works

My goal is to get the anodising working in a very small setup before investing any more money in it - hence the clothing dye. I don't care if it fades, etc - as long as it works a little.

Okay - so I'll pick up a cheap water heater and get the temp to about 72F.

With the electrolyte I'll try it at a lower concentration - The bubbles are really coming off of it - its like an airstone - would that indicate it is indeed disolving the surface faster then its being created?

If you guys help me sort this out I'll send each of ya a wee token!