Thread: ano fading....
View Single Post
  #1 (permalink)  
Old 09-01-2004, 03:09 PM
Sid03 Sid03 is offline
Amateur Metal Finisher
 
Join Date: Dec 2003
Posts: 153
Sid03
Default ano fading....

Did some parts a couple months ago. Parts are half red and half orange. The orange seems fine(although may be harder to notice since its a liter color) but the red is fading. Actually, it seems to rub off. If you rub it a bit with your finger, you will get a small amount of pinkish/red on your finger.

....bad sealant?