Combined powder coat & anodize
This is a dual forum post, involving powder coating & anodizing. I’ve posted this on the Anodizing forum as well. Now that I’ve got these two figured out, it’s time to do some real parts.
I’ve got a cast aluminum part that has a steel part embedded. I’m planning to mask the steel (w/Caswell liquid Mask-It), anodize the aluminum, then mask the aluminum, and powder coat the steel. (or the other way around).
Is powder coat affected by an anodize bath? (25% sulfuric acid)
If so, I can mask it off, but then is the PC surface finish affected by the masking agent?
Best to PC first, or anodize first?
Does anyone see other problems with this?