The problem you may face with heat is the different thermal expansion between metallic aluminum (expands a lot) and the ceramic anodize (expands a little). This can produce a substantial mechanical stress on the anodize and crack it. I don't know the temperature where this becomes a problem. NeoMoses thinks its around 300 deg. F..