Thanks guys!

Concensus from both forums is to anodize first, then PC.

There’s a potential issue w/different thermal expansion rates between raw aluminum & the anodize layer, so I’ll have to test that out first. If so, I’ll reduce oven temp to recommended minumum & post the results.