My oven is built out of angle iron, and cement board and measures 6ft wide, 3 feet deep and 6 feet high. For heating I have used for over 2 years 4 triple Mr Heater infrared elements with great success. The next oven I will use sheetmetal and have it well insulated, but this has worked great for me for 2 years.