I too have learned alot from reading this forum. Having some trouble with the little marks. My plater called them air bubbles. She, (yes she) said that I may be taking too much metal off with my sanding. Been starting with coarse moving to fine dry. Then, wet steps. I'm not seeing the orange peel look until I start polishing. I initially started with brown. I t was like I was just putting in this look. So, tried black. With alot of work, it seems to come out some. When I think I've worked them out and move to white, the orange peel starts shinin too. I am working on stock Harley Davidson aluminum parts. The plater says she'll build up the copper to cover these. However, I would like to not submit my work with these in. Obviously, for polished only pieces this won't do. Any further discussion on this would help.