My plater does the triple chrome. She says the copper will fill the gas bubbles. However, it will be more cost effective for me to deliver withot these. She dosen't have to "build up" the copper to cover. I just did a test piece using the abrasive wheel compound 120 then 240. Then went to 400 and 600 dry. Then 800-1000 wet. Went to the black compound and then to white. NO GAS BUBBLES! I'm encouraged! Think my problem has been not doing a good enough job sanding.