Yes.
Like Neilfj said; The top most parts of the pore structure have broken off, taking most or some of the sealant with it. With no sealing the dye will "fade" (actually its coming out). If you soak these parts in alcohol (any kind) or even water, does the dye come out? If any does, you lost your seal.