Well thank you for your help with the power supply issues. I have built a holder with a selection of resistors and a fan to keep them cool. So I have come to realize that I am going to be living with the resistors. At the lower current settings it makes the meter very constant and able to control it easier. So yes it may have been a blessing in disguise.
I have since found out that 99% of my problems have been using the wrong information to set the power supply in the first place. The manual I found has a lot of discrepancies that are at the cause. The biggest is the setting for ACID copper. Should read 1 amp for every 16 sq" not 1 amp for 10-30 sq".
It is great, using correct info