In a simple answer..... yes and no.
Yes they can be mixed without problems as long as chemistry is similar.
No they don't mix like liquids to give another shade. If you have any 2 powders in your shop mix them 50/50 and shoot on scrap, you will see.You can change base coat color to change the shade of the top coat or mix and match for different effects.
|