I just reread the post again and it showed up on the white prior to second coat? Correct?
If this is the case then its a prep problem.I've had bike necks bleed oil outta the welds after prebaking 3 or 4 times.

I'm not saying its oil but something left on surface prior to coating. I would strip it and start from scratch.