here is an experience i had.... i used almost chrome on a piece and emptied the cup when i was finished, but did not blow out the gun and nozzle parts. i then placed a cup of black on the gun and shot it on a scrap piece of metal. after curing, i found the finish to be a metalic black. something looking like black with silver metal flake. it looked kinda cool.