I sure did mix as instructed. The temperature might not have been quite there because the parts were anodized and I was preparing the sealer longer than expected, but it wasn't far off the mark.
That was going to be my test next time I ran the system. It's good to know that boiling water is just as good in small scale parts. That said, is it better to use Nickel acetate sealants on parts with large surface areas?