Welcome to the forum  Bolts depends on how many.If it's only a few at a time I just wrap a wire around the threads then wrap the threads with fiberglass tape and then bend end of wire into hook shape for hanging.If it's alot I use sheet metal with holes in it to place the bolts in to.Or some times make metal blocks with lots of threaded holes and just screw the bolts in just short of all the way.
As for IR lamps you'll have to wait for an IR guy to chime in.I prefer ovens but IR works fine too.
|
Thanks for the reply Dale. I plan on curing smaller parts in an electric oven. But for the larger parts maybe trying an ir lamp, until I can get around to building a larger oven.