Oven Cleaner Overspray
O.k, So I got finally got motivated to polish the frame of my '02 GSXR. Done my research on frame polishing for about a month. I use oven cleaner to strip the anodize off....One problem, I got in a rush and didn't mask off the parts I didn't want to be stripped. Now I have parts of my frame that I didn't want to have to polish due to the problem of getting a wheel in tight spots that are now stripped of anodize and I cant possibly get any kind of polishing wheel to those spots. I now have major visual spots on the frame and other areas that are two, three diffrent colors from the oven cleaner. What is my best course of action now to make those spots look even half way unnoticable. I am thinking maybe a dremel tool with a small wire wheel at moderate speed? Anyone else do this to themselves before and have any comments, suggestions?
|