Default Clear coat problem

Ive been using the hobby gun for a lotta pieces and parts and I am now starting to try clear over a color. After the first coat of a standard color is cured I try to spray clear and not enough sticks to coat the part. I thought up two reasons. One, the gun is too weak to charge the clear enough to stick because of the thickness of the first coat, and two, not a good ground but I checked that. Also I tried spraying when the part was hot and that worked pretty good, but I want to be able to do it the other way.

If anyone is not having this problem or if you can help me that would be great,

Thaks
Evan