was playing arround today with the vinyl cutter and thought i would try it.
note the preping on the part wasn't the best. and the time in the tank was extremly short. plus my agitaor pump broke half way in. so now i need to try and find a prop for it.





oh yeah what a bitch to get the vinyl off afterwards. but do's leave nice sharp lines.