It looks like whatever was on it originally hasn't been completely removed, an outside radius is an odd place to see this though. I'm assuming that your rinsing between steps is complete and through. The edges like that can get work hardened if they were under severe mechanical stress during whatever machining was done, too bad you don't know where its been.

Maybe M_D has seen this before and can shed some light on it.