View Single Post
  #4 (permalink)  
Old 11-25-2004, 09:53 PM
lastone75 lastone75 is offline
Amateur Metal Finisher
 
Join Date: Apr 2003
Posts: 51
lastone75
Send a message via AIM to lastone75
Default

the blemish isn't an issue with 8AWG

the problem is the 16AWg is a little to flimsy. and with the agitaor the parts tend to hit each in the tank. only one of the parts i do draws over 5 amps. but to use the smaller gauge i would have to still hook up my old way to to keep them still in the tank. so to avoid using 2 wire to hang a part i just use the heavier wire. with the bigger wire the blemish isn't to bad and in most cases very easy to hide. it leave a mark maybe twice the size the 16AWG leaves.

but it's all about what easier to use for the user.