No.
I have experience with finishing 12L14 with most chemical conversion methods, from hot caustic blueing to cold blue and black oxide. I haven't tried Caswell's, but I have no reason to believe it would be any different. This alloy is quite easy to finish, it took every finish, including Parkerizing with no difficulties. The miniscule lead content of 12L14 has no effect on the finishing.
|