Electroless Nickel's main advantage over regular nickel is that it plates a completely even layer.
With regular electroplating, where areas of the part are closer to the anode, those areas tend to build up a slighty thicker layer of metal. Not so with electroless.
25 microns (1/1000") for that application would be fine. Yes, that's approx 1 hour plating time.
What are the dimensions of the barrels?
What are they made of?
|