I would like to ask a question about the flash copper.
Just to back up a bit. I have a 15 gallon tank of flash copper and at one time it was working great. Meaning great throwing as well as a nice color. Now I am getting black spots as well as spots that are not plating or even not throwing onto areas in front of the anodes. I do not know what happened? Any ideas?
To change the subject, I have tried the silver paint on a leaf and it worked good. The only problem I had was getting the current to go low enough. But I will try again soon.
On bare steel the flash copper works great. On a part that I have stripped the nickel off I am running into problems. I ran the solution through a filter with activated charcoal thinking I had contamination. But the results on the bare steel tells me it is not that.