Has anyone used the Cerakote Exotic Color coatings? I've read the info page on the Caswell site and it is unclear to me whether or not this product is a true (or perhaps a better word would be "traditional") power coat. I don't see anything in the instructions about baking the product once applied. It says that "Parts will be tack free after approximately 35 minutes." which to me sounds like some sort of paint. Is this product a liquid or a powder?
Aside from the details of what it is and how it is applied, has anyone used it? I am considering if for an auto restoration for some valve covers, specifically a set of valve covers on a 1600 cc VW aircooled engine. They probably run somewhat hotter than watercooled engine valve covers but I think they should stay under the 800 ºF rating of this product.
Thanks in advance for any insight anyone can provide.
Scott
|