I use the green hi-temp tape and have no problems with. Yes, once the part is fully curred it might wrinkle some but it does it job. I use the green hi -temp with no problems on 1, 2 and 3 coat applications. Stick with the hi temp. It might peel and curl when done but will come off eaisly. Tape is used for protecting those areas when coating that you dont want the powder to go on. If your doing a two or three stage coating and the tapes peeling/lifting then I think the user has gotta be over curing there first coating.
Just my opinion as I have had no problems with the hi-temp g. tape.