I am new to the polishing hobby but have always wanted to do it. So after reading the caswell handbook thoroughly i had enough guts to attempt some polishing. I decided that i wanted to do my turbo housing for my truck. I took some pics from the beginning and i am going to keep posting them as time goes on. Maybe we can all learn from this? Maybe i just want to show off! LOL! Anyway here ya go!!



This was the pic in the beginning with nothing done but some experimenting on the inlet. Stage 1



This was a shot after i hit the housing with a dremel to knock down the casting lines and bumps. I also ground down the numbers. I think i want to keep the mitsubishi word. I don't know why but...?? Stage 2

I think there will be more stage two to come. This seems to be the longest step. I need to find some sorta pointy bit to get in the recessed area? How do those bobs work?